De-laminated prindle 16

the side on one of the hull of my prindle 16 is de-laminade and it crack to the top were is connect to the deck .
the de-lamination is covering almost all side of the hull and the fibre glass behind is soft .
How can I fix it ?
Cross your fingers and use the method in the article on the home page.

--
Greenville SC

Offering sails and other go fast parts for A-class catamarans
--
Look for a newer set of hulls, it can be very dangerous if you sail in the ocean. We have had 2 boats break up due to similar problems while sailing off South East Florida. There is an old expression 'IF THE HORSE IS DEAD, GET OFF'
ilpellegrinothe side on one of the hull of my prindle 16 is de-laminade and it crack to the top were is connect to the deck .
the de-lamination is covering almost all side of the hull and the fibre glass behind is soft .
How can I fix it ?