[quote=shipchips1]I am using 105 and 206 for my deck and various other repairs. I like the slow set time, it gives the resin a chance to creep into the old foam and glass to give a better bond and I don't have to race to get it all done. With the syringes remember to leave some resin with a wire in it and the next day when it is hard you just pull the wire and the hardend resin pops right out.
On all my other repairs I wet out with the same mix for the same reasons, this will give a better bond.
One of the things you are paying extra for with the West System is its ease of use, to me it is worth the money, one less thing I need to worry about.
good luck
Jim[/quote]