  • Ok maybe a dumb question, but I am completly new to sailing... Just bought an 85 P18, how do I check for soft spots? I mean is it as abvious as the word implies, literally soft spots somewhere on the fiber??

    Thanks
  • Yes it is really that simple. Just work your way around the boat pushing on the hull every few inches. If you feel no motion it is probably solid. If the glass moves under you hands you are typically looking at a soft spot. If you hear anything crunch you are definitely looking at a spot in need of repair. Don't be gentle, the p18 is a tough boat and if you manage to break something checking for soft spots it was going to break anyway the first time you put the boat on the water.
  • they tend to be on the deck lids(top) of hulls, especially foreward of the crossbars where people have a tendancy to sit/stand...you will hear the "crunch" sound when you put some pressure on it. check the sides of the hulls too by pressing with your fingers all over it. these will give a hollow sound like a blister when you tap on them compared to the surrounding areas. it's not a difficult repair if you find some.

    --
    Check out "Prindle Sailors" on Facebook!
    bill harris
    hattiesburg, mississippi
    prindle 16- "BLUE RIBBON"
    --
  • One more for the Prindle folks. Since I'm in the process of buying are P16's prone to having a common delam spot besides just fore of the crossbar?

    It seems that most repairs I've seen have been to the top deck how common are delam issues on the vertical parts of the hull? Are the sides of the hull the same sandwich construction as the deck lid?

    --
    Bob Miller
    1983 P16 Sail # 7312
    "Miller Time" A work in progress; out of the water for 16 years
    Barnegat Bay NJ
    Beach Cat Lesson #1 - A free cat isn't
    Find more Prindles on Facebook https://www.facebook.com/groups/173120656090532/
    --
  • sides are foam core also...it useually takes a hard shot to the glass to make a delam on the sides but i have seen a few with huge delams on the exterior sides by the for crossbar...but these are super obvious. you will see some with wavey sides on the inside of the hulls, this is from being flipped a bunch and people standing/bouncing on them to right the boat, they may not be soft though, just "wavey".

    --
    Check out "Prindle Sailors" on Facebook!
    bill harris
    hattiesburg, mississippi
    prindle 16- "BLUE RIBBON"
    --
  • Our P18 has some soft spots on the inside of the hull, so it definitely happens! They are just aft of the forward beam. about 3-5 inches lower then the hull lip. nice winter project...

    --
    Stefan, Denmark.
    H14,H16,P16,P18,SC17,N5.8
    Team StaySail
    http://www.staysail.eu
    --
  • The only soft spot on my '82 P18 were top of starboard hull between the front crossbar and the port.

No HTML tags allowed (except inside [code][/code] tags)

  • Options
  • 0 users

This list is based on users active over the last 60 minutes.

Upcoming Beachcats Events

VIEW FULL CALENDAR

No upcoming events.