I need to paint some contrasting index marks on gelcoat (mostly rudders, centerboards and a bit of deck work).
Will Krylon work?
Do I need to prep the surface beyond cleaning it with acetone first?
Should I seal it afterward?
I do not have any wax, polish or speed goo on the gelcoat now.
Sheet In!
--
Sheet In!
Bob
_/)_____/)_/)____/)____/)_____/)/)__________/)__
Prindle 18-2 #244 "Wakizashi"
Prindle 16 #3690 "Pegasus" Sold (sigh)
AZ Multihull Fleet 42 member
(Way) Past Commodore of Prindle Fleet 14
Arizona, USA
--
Paint suggestions
-
- Rank: Chief
- Registered: Apr 19, 2011
- Last visit: Nov 20, 2024
- Posts: 1460
-
- Rank: Lubber
- Registered: Jul 06, 2008
- Last visit: Mar 23, 2016
- Posts: 94
I painted the bottoms of my hulls with several coats of 2 part epoxy paint (West Marine) like 3 years ago. Prep was a light sanding with wet/dry 600 and acetone. the paint has held up exceptionally well with beaching the boat in non-rock ridden sand.
Krylon won't last. Consider using a small batch of West System Epoxy and pigment/dye (it can be dyed to get rid of yellow overtones). Many folks use this as the sacrificial keel coat every five years or so and dye it to match their hulls. I'm guessing its almost the same as what I used. Just tape off your marks roller it on with the ultra low foam roller (ask the guys at West Marine and they will hand you the correct roller) and "tip" to get rid of orange peel. Second coat should be before first coat hardens. Remember this coat will be slightly thicker that krylon, so don't get too nutty or your dagger boards will be tighter.
--
nacra inter-18
CNBP
-- -
- Rank: Mate
- Registered: Dec 18, 2009
- Last visit: Oct 10, 2019
- Posts: 117
I also used a two part epoxy from West Marine and got a very good result. If your painting over gelcoat make sure you sand with a 120 to 150 grit sandpaper and use a primer before placing you top coat (the primer is also available at West Marine).
--
Scott
ARC 21
Prindle 18
Annapolis, Maryland
-- -
- Rank: Mate
- Registered: Oct 11, 2011
- Last visit: May 14, 2014
- Posts: 104
Do they make a epoxy dye that is both UV and can be tinted blue? I have some above the waterline issues that need to be addressed and before i repaint the whole cat I want to be sure it floats.
--
Bob Miller
1983 P16 Sail # 7312
"Miller Time" A work in progress; out of the water for 16 years
Barnegat Bay NJ
Beach Cat Lesson #1 - A free cat isn't
Find more Prindles on Facebook https://www.facebook.com/groups/173120656090532/
-- -
- Rank: Lubber
- Registered: May 05, 2010
- Last visit: Jun 06, 2012
- Posts: 33
I used the interlux 2000 2 part epoxy paint avaliable at west marine. I love the outcome. I am sure it can be tinited blue, but no idea to acutally how, talk to the guys at west and they can point you in the right direction. as far as prep. i sanded first, was with acetone, sand again, wash with acetone, be sure to use gloves. have fun -
- Rank: Chief
- Registered: Apr 19, 2011
- Last visit: Nov 20, 2024
- Posts: 1460
Wow- pretty solid West Marine response.
Thanks all!
--
Sheet In!
Bob
_/)_____/)_/)____/)____/)_____/)/)__________/)__
Prindle 18-2 #244 "Wakizashi"
Prindle 16 #3690 "Pegasus" Sold (sigh)
AZ Multihull Fleet 42 member
(Way) Past Commodore of Prindle Fleet 14
Arizona, USA
-- -
- Rank: Mate
- Registered: Jul 06, 2008
- Last visit: Jul 19, 2018
- Posts: 986
I wish the Interlux had a good lime green.
--
Dustin Finlinson • Magna, UT
Member: Utah Sailing Association
1982 Prindle 18
1986 Hobie 17
1982 Prindle 16
1980 Prindle 16(mostly)
1976 Prindle 16(mostly)
Check out "Prindle Sailors" on Facebook.
--
Users on-line
- 0 users
This list is based on users active over the last 60 minutes.