Even if your injection does not fully fix your problem it will improve it a lot and you can still do some surface glass if you think you need it.
I did injection on a Hobie 17 and it did not go well at all but it is still 80 stronger than it was before I started.
--
Dustin Finlinson • Magna, UT
Member: Utah Sailing Association
1982 Prindle 18
1986 Hobie 17
1982 Prindle 16
1980 Prindle 16(mostly)
1976 Prindle 16(mostly)
Check out "Prindle Sailors" on Facebook.
--
Prindle 16 in a bad state of repair
-
- Rank: Mate
- Registered: Jul 06, 2008
- Last visit: Jul 19, 2018
- Posts: 986
-
- Rank: Lubber
- Registered: Sep 25, 2015
- Last visit: Oct 08, 2015
- Posts: 9
OK,
Update on my Prindle. The injection method did not really produce the result that I had hoped for. Some parts are really firm but some are still soft and then when I sat on them it cracked again. Will try a layer of glass mat over the top and see how that goes. Hopefully with both it will hold up.
Cheers Rob